Beilstein J. Nanotechnol. 2021, 12, 366–374, doi:10.3762/bjnano.12.30
Figure 1: SEM images of the morphological evolution of strained Mn wetting layers with different thickness af...
Figure 2: X-ray diffraction pattern of the 9 ML thick Mn wetting layer, upon annealing at 650 °C for 15 min. ...
Figure 3: SEM images of the surface after deposition of 4.5 ML Mn on Ge(111) wafer and annealing at 650 °C fo...
Figure 4: (a) SEM image of a typical NW, ≃700 nm long, obtained by deposition of a 4.5 ML thick Mn film follo...
Figure 5: EDX elemental map (Kα line), carried out on a cross-section of a NW on the surface of the 4.5 ML th...
Figure 6: Cross-section image of the NW along its length. (a) TEM image of a 1.15 μm long NW capped with a Pt...
Figure 7: (a) Length (t) and width (s) of Mn5Ge3 islands, formed on the sample surface of the 4.5 ML thick Mn...