Beilstein J. Nanotechnol. 2019, 10, 238–246, doi:10.3762/bjnano.10.22
Figure 1: Measured XRR spectra (left column), fitted curves (middle column) as well as silver or gold layer d...
Figure 2: Left - Atomic concentration of Te atoms in the sandwich-like silver sample (black curve) as well as...
Figure 3: (a,b) Imaginary part of the permittivity for 35 nm-thick silver (a) and gold (b) layers deposited o...
Figure 4: Left – Comparison of imaginary parts of the permittivity for 35 nm-thick Ag layers deposited on top...
Beilstein J. Nanotechnol. 2018, 9, 66–76, doi:10.3762/bjnano.9.9
Figure 1: XRD spectra of the investigated silver films. The intensity of each spectrum was normalized to the ...
Figure 2: 3 × 3 µm2 AFM scans of 35 nm thick silver films. (a) Non wetted film, (b) Ge wetted, not annealed f...
Figure 3: Measured XRR spectra (left column), fitted curves (middle column) as well as silver layer density p...
Figure 4: Scheme of the structure of the silver layers grown on Ge wetting films before (left) and after (rig...
Figure 5: Imaginary part of permittivity for 35 nm thick Ag films deposited on 2 nm thick Ge wetting layer an...
Figure 6: Transmission spectra of non-annealed (left column) and annealed (right column) Ag layers deposited ...
Figure 7: (a) Transmission spectra of Ge/Ag multilayer structure with total thickness of 20 nm. (b) Imaginary...
Figure 8: Raman spectra of 20 nm thick Ag layers deposited on 5 nm thick Ge wetting films.