Beilstein J. Nanotechnol.2012,3, 692–702, doi:10.3762/bjnano.3.79
produced by vaporization from a resistively heated iron wire (current 2.7 A, diameter 250 μm, purity 99.95%, Goodfellow, USA) in a H2/Ar (7/93 mol ratio) flow of 480 cm3·min−1 inside an aluminiumoxide (Al2O3) tube (inner diameter 16 mm). Particles formed and grew through vapor nucleation–condensation and
PDF
Figure 1:
SEM images of as-prepared SWCNT networks dry-transferred onto the aluminium substrate. From top lef...
Beilstein J. Nanotechnol.2012,3, 192–197, doi:10.3762/bjnano.3.21
distinct pattern of line vacancies reflected by the underlying lattice structure. Consequently, by the creation of triangular patches in a 6√3×6√3R30° superstructure, the polar-stabilization requirements are met.
Keywords: aluminiumoxide; metal oxide surfaces; noncontact atomic force microscopy (NC-AFM
PDF
Figure 1:
(a) Ball model of the MgAl2O4 stacking sequence in the [111] direction showing one repeat unit of 4...